Nylon 66 is a 33% glass fiber reinforced heat stabilized impact modified
https://forever-plastics.en.made-in-china.com/product/rJwRvlcdZpWD/China-Nylon-PA6-GF33-PA66-Granules-PA6-with-30GF-Polyamide-PA66-30-GF-PA6-Material.html Heat-conducting nylon
Product Description | |||
5133 HS is a 33% glass fiber reinforced, heat stabilized, impact modified, Nylon 66 suitable for injection molding. It offers excellent balance of mechanical, thermal and chemical properties; exceptional toughness, stiffness, and dimensional stabili 5133 HS is available in UV stable, custom colors, and impact modified grades. It also has excellent chemical resistance to greases, oils, and other hydrocarbons. Typical applications include hardware and automotive under the hood components. |
|||
General | |||
Form Resin Pellets | |||
Filler 33 % Glass Fiber | |||
Outdoor Chemical Resistant Good Dimensional | |||
Feature | Enhanced Stiffness Good Thermal | Ductile Grease Resistant Hydrocarbon Resistant High Impact |
|
Fuel Resistant | |||
Uses | Automotive Under The Hood |
||
Physical Nominal Value Test Method | |||
Density / Specific Gravity 1.35 g/cm³ ASTM D792 | |||
Molding Shrinkage, Flow 0.50 % ASTM D955 | |||
Molding Shrinkage, Across Flow 0.80 % ASTM D955 | |||
Water Absorption(24 hr) 0.50 % ASTM D570 | |||
Rockwell Hardness, R-Scale 122 ASTM D785 | |||
Mechanical Nominal Value Test Method | |||
Tensile Strength(51 mm/min) 165 MPa ASTM D638 | |||
Tensile Elongation, Break(51 mm/min) 3.0 % ASTM D638 | |||
Flexural Modulus(51 mm/min) 8000 MPa ASTM D790 | |||
Flexural Strength(51 mm/min) 230 MPa ASTM D790 | |||
Notched Izod Impact(6.35 mm) 210 J/m ASTM D256 | |||
Thermal Nominal Value Test Method | |||
Deflection Temperature Under Load, Unannealed ASTM D648 | |||
0.45 MPa 260 °C | |||
1.8 MPa 240 °C | |||
Melting Temperature 258 °C DSC | |||
Processing | Nominal Value | ||
Drying Temperature<Injection> | 71 - 82 °C | ||
Drying Time<Injection> | 4.0 - 6.0 hr | ||
Rear Temperature<Injection> | 266 - 282 °C | ||
Middle Temperature<injection> | 277 - 293 °C | ||
Front Temperature<Injection> | 288 - 304 °C | ||
Nozzle Temperature<Injection> | 282 - 302 °C | ||
Processing Temp, Melt<Injection> | 288 - 304 °C | ||
Mold Temperature<Injection> | 77 - 88 °C | ||
Injection Rate<Injection> | Fast | ||
Back Pressure<Injection> | 0.138 - 0.345 MPa | ||
Cushion<Injection> | 1.59 - 6.35 mm | ||
Screw L/D Ratio<Injection> | 16.0:1.0 | ||
Screw Compression Ratio<Injection> | 3.0:1.0 |